Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 2571 Phenolic, Granular, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Woodflour Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 2571 Phenolic, Granular, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized under component file E40654. 02571 is available in black or brown color.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.620 g/cc
0.0224 lb/in³
ASTM D1895
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
Water Absorption 0.40 %
0.40 %
ASTM D570
Linear Mold Shrinkage 0.0048 cm/cm
0.0048 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 87
87
ASTM D785
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Elongation at Break 0.69 %
0.69 %
ASTM D638
Tensile Modulus 8.30 GPa
1200 ksi
ASTM D638
Flexural Strength 90.0 MPa
13100 psi
ASTM D790
Flexural Modulus 8.50 GPa
1230 ksi
ASTM D790
Compressive Strength 212 MPa
30700 psi
ASTM D695
Izod Impact, Notched 0.169 J/cm
0.317 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.191 J/cm²
0.909 ft-lb/in²
ASTM D256
Impact 109
109
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Thermal Conductivity 0.370 W/m-K

@Temperature 100 °C
2.57 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 205 °C
401 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 175 °C
347 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Oxygen Index 25.5 %
25.5 %
ASTM D2863
Shrinkage 0.173 %
0.173 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 8.00e+11 ohm-cm
8.00e+11 ohm-cm
ASTM D247
Dielectric Constant 5.2
5.2
ASTM D150
Dielectric Strength 14.3 kV/mm
363 kV/in
Short Time; ASTM D149
Dissipation Factor 0.047
0.047
ASTM D150
Arc Resistance 134 sec
134 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638