Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 3303 Phenolic, Granular, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral/Flock Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 3303 Phenolic, Granular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Plenco 03303 is a renumber of Plaslok 5303. Plenco 03303 is a two-stage, mineral and flock-filled phenolic molding compound offering excellent electrical insulating properties. It can be processed by compression, transfer or injection molding . It is UL recognized under file E40654.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.610 g/cc
0.0220 lb/in³
ASTM D1895
Density 1.54 g/cc
0.0556 lb/in³
ASTM D792
Water Absorption 0.32 %
0.32 %
ASTM D570
Linear Mold Shrinkage 0.0084 cm/cm
0.0084 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 83
83
ASTM D785
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ASTM D638
Elongation at Break 0.77 %
0.77 %
ASTM D638
Tensile Modulus 9.80 GPa
1420 ksi
ASTM D638
Flexural Strength 82.0 MPa
11900 psi
ASTM D790
Flexural Modulus 8.70 GPa
1260 ksi
ASTM D790
Compressive Strength 182 MPa
26400 psi
ASTM D695
Izod Impact, Notched 0.193 J/cm
0.362 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.183 J/cm²
0.871 ft-lb/in²
ASTM D256
Impact 114
114
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 201 °C
394 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 168 °C
334 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Shrinkage 0.34 %
0.34 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 3.10e+11 ohm-cm
3.10e+11 ohm-cm
ASTM D247
Dielectric Constant 5.5
5.5
ASTM D150
Dielectric Strength 6.20 kV/mm
157 kV/in
Step by Step; ASTM D149
9.40 kV/mm
239 kV/in
Short Time; ASTM D149
Dissipation Factor 0.068
0.068
ASTM D150
Arc Resistance 180 sec
180 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638