Plenco 4311 Phenolic, Granular, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 4311 Phenolic, Granular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized under component file E40654. 04311 is available in black or brown.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.710 g/cc
0.0257 lb/in³
ASTM D1895
Density 1.48 g/cc
0.0535 lb/in³
ASTM D792
Water Absorption 0.267 %
0.267 %
ASTM D570
Linear Mold Shrinkage 0.0083 cm/cm
0.0083 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 79
79
ASTM D785
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ASTM D638
Elongation at Break 0.78 %
0.78 %
ASTM D638
Tensile Modulus 9.10 GPa
1320 ksi
ASTM D638
Flexural Strength 89.0 MPa
12900 psi
ASTM D790
Flexural Modulus 8.00 GPa
1160 ksi
ASTM D790
Compressive Strength 177 MPa
25700 psi
ASTM D695
Poissons Ratio 0.34
0.34
ASTM D638
Shear Modulus 3.40 GPa
493 ksi
Calculated
Izod Impact, Notched 0.155 J/cm
0.290 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.165 J/cm²
0.785 ft-lb/in²
ASTM D256
Impact 87
87
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C

@Temperature 40.0 - 130 °C
27.8 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.490 W/m-K

@Temperature 100 °C
3.40 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 206 °C
403 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 167 °C
333 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
Oxygen Index 29.4 %
29.4 %
ASTM D2863
Shrinkage 0.288 %
0.288 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 4.10e+11 ohm-cm
4.10e+11 ohm-cm
ASTM D247
Dielectric Constant 5.2
5.2
ASTM D150
Dielectric Strength 7.70 kV/mm
196 kV/in
Step by Step; ASTM D149
11.0 kV/mm
279 kV/in
Short Time; ASTM D149
Dissipation Factor 0.059
0.059
ASTM D150
Arc Resistance 159 sec
159 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638