Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 4327 Phenolic, Granular, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Resole, Mineral Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 4327 Phenolic, Granular, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 04327 is a heat resistant mineral filled phenolic molding compound offering excellent cosmetic characteristics and improved heat resistant properties. PLENCO 04327 is not intended for electrical insulating applications. 04327 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.680 g/cc
0.0246 lb/in³
ASTM D1895
Density 1.51 g/cc
0.0546 lb/in³
ASTM D792
Water Absorption 0.36 %
0.36 %
ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 83
83
ASTM D785
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ASTM D638
Elongation at Break 0.91 %
0.91 %
ASTM D638
Tensile Modulus 8.90 GPa
1290 ksi
ASTM D638
Flexural Strength 85.0 MPa
12300 psi
ASTM D790
Flexural Modulus 8.40 GPa
1220 ksi
ASTM D790
Compressive Strength 200 MPa
29000 psi
ASTM D695
Izod Impact, Notched 0.156 J/cm
0.292 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.196 J/cm²
0.933 ft-lb/in²
ASTM D256
Impact 102
102
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 53.0 µm/m-°C

@Temperature 40.0 - 130 °C
29.4 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 205 °C
401 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
ASTM D648
Shrinkage 0.284 %
0.284 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 4.20e+13 ohm-cm
4.20e+13 ohm-cm
ASTM D247
Dielectric Constant 5.7
5.7
ASTM D150
Dielectric Strength 11.6 kV/mm
295 kV/in
Short Time; ASTM D149
Dissipation Factor 0.033
0.033
ASTM D150
Arc Resistance 86 sec
86 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638