Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 4527 Phenolic, Granular, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Resole, Mineral/Flock Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 4527 Phenolic, Granular, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 04527 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength, and resistance to cracking in a wet-dry environment. UL recognized under component file E40654. 04527 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.630 g/cc
0.0228 lb/in³
ASTM D1895
Density 1.59 g/cc
0.0574 lb/in³
ASTM D792
Water Absorption 0.56 %
0.56 %
ASTM D570
Linear Mold Shrinkage 0.0034 cm/cm
0.0034 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 67
67
ASTM D785
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ASTM D638
Elongation at Break 1.11 %
1.11 %
ASTM D638
Tensile Modulus 9.50 GPa
1380 ksi
ASTM D638
Flexural Strength 83.0 MPa
12000 psi
ASTM D790
Flexural Modulus 9.20 GPa
1330 ksi
ASTM D790
Compressive Strength 163 MPa
23600 psi
ASTM D695
Izod Impact, Notched 0.271 J/cm
0.508 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.251 J/cm²
1.19 ft-lb/in²
ASTM D256
Impact 147
147
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 210 °C
410 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 240 °C
464 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
Oxygen Index 35 %
35 %
ASTM D2863
Shrinkage 0.40 %
0.40 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 4.90e+11 ohm-cm
4.90e+11 ohm-cm
ASTM D247
Dielectric Constant 7.9
7.9
ASTM D150
Dielectric Strength 6.90 kV/mm
175 kV/in
Short Time; ASTM D149
Dissipation Factor 0.12
0.12
ASTM D150
Arc Resistance 184 sec
184 sec
ASTM D495
Comparative Tracking Index 200 V
200 V
ASTM D3638