Plenco 50125 PET, Pellet, Injection Molded, White  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 50125 PET, Pellet, Injection Molded, White  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 50125 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white only.Information supplied by PlencoPlenco discontinued their PET product line in 2005.
Physical Properties Metric English Comments
Density 1.83 g/cc
0.0661 lb/in³
ASTM D792
Water Absorption 0.050 %
0.050 %
ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ATM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 144.3 MPa
20930 psi
ASTM D638
Elongation at Break 1.69 %
1.69 %
ASTM D638
Tensile Modulus 13.13 GPa
1904 ksi
ASTM D638
Flexural Yield Strength 179.1 MPa
25980 psi
ASTM D790
Flexural Modulus 10.82 GPa
1569 ksi
ASTM D790
Compressive Yield Strength 193 MPa
28000 psi
ASTM D695
Izod Impact, Notched 0.750 J/cm
1.41 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 247 °C
477 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.47 mm
V-0

@Thickness 0.0579 in
Electrical Properties Metric English Comments
Electrical Resistivity 3.40e+16 ohm-cm
3.40e+16 ohm-cm
ASTM D257
Dielectric Constant 3.6

@Frequency 1e+6 Hz
3.6

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 14.8 kV/mm
376 kV/in
Short Time; ASTM D149
Dissipation Factor 0.011

@Frequency 1e+6 Hz
0.011

@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 175 V
175 V
ASTM D3638