Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 50130 PET, Pellet, Injection Molded, Black  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 50130 PET, Pellet, Injection Molded, Black  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 50130 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in natural and black.Information supplied by PlencoPlenco discontinued their PET product line in 2005.
Physical Properties Metric English Comments
Density 1.73 g/cc
0.0625 lb/in³
ASTM D792
Water Absorption 0.050 %
0.050 %
ASTM D570
Linear Mold Shrinkage 0.00090 cm/cm
0.00090 in/in
ATM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 137.9 MPa
20000 psi
ASTM D638
Elongation at Break 1.65 %
1.65 %
ASTM D638
Tensile Modulus 11.41 GPa
1655 ksi
ASTM D638
Flexural Yield Strength 206.1 MPa
29890 psi
ASTM D790
Flexural Modulus 10.94 GPa
1587 ksi
ASTM D790
Compressive Yield Strength 164.7 MPa
23890 psi
ASTM D695
Izod Impact, Notched 0.680 J/cm
1.27 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.47 mm
V-0

@Thickness 0.0579 in
Electrical Properties Metric English Comments
Electrical Resistivity 5.9566e+17 ohm-cm
5.9566e+17 ohm-cm
ASTM D257
Dielectric Constant 3.4

@Frequency 1e+6 Hz
3.4

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 16.1 kV/mm
409 kV/in
Short Time; ASTM D149
Dissipation Factor 0.011

@Frequency 1e+6 Hz
0.011

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 40 sec
40 sec
ASTM D495
Comparative Tracking Index 200 V
200 V
ASTM D3638
Copyright © lookpolymers.com All Rights Reserved