Plenco 51015 PET, Pellet, Injection Molded, Black  (discontinued **)

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 51015 PET, Pellet, Injection Molded, Black  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 51015 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL listed.Information supplied by PlencoPlenco discontinued their PET product line in 2005.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ASTM D792
Water Absorption 0.070 %
0.070 %
ASTM D570
Linear Mold Shrinkage 0.0015 cm/cm
0.0015 in/in
ATM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 96.3 MPa
14000 psi
ASTM D638
Elongation at Break 1.61 %
1.61 %
ASTM D638
Tensile Modulus 6.79 GPa
985 ksi
ASTM D638
Flexural Yield Strength 127.4 MPa
18480 psi
ASTM D790
Flexural Modulus 6.43 GPa
933 ksi
ASTM D790
Compressive Yield Strength 154.5 MPa
22410 psi
ASTM D695
Izod Impact, Notched 0.390 J/cm
0.731 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 206 °C
403 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
Electrical Properties Metric English Comments
Electrical Resistivity 2.20e+16 ohm-cm
2.20e+16 ohm-cm
ASTM D257
Dielectric Constant 2.9

@Frequency 1e+6 Hz
2.9

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 15.8 kV/mm
401 kV/in
Short Time; ASTM D149
Dissipation Factor 0.011

@Frequency 1e+6 Hz
0.011

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 80 sec
80 sec
ASTM D495
Comparative Tracking Index 200 V
200 V
ASTM D3638