Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 5350 Phenolic, Granular, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral/Graphite Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 5350 Phenolic, Granular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 05350 is a mineral and graphite filled phenolic molding compound, developed for seal applications. PLENCO 05350 offers excellent dimensional stability, lubricity, and low abrasion properties. 05350 is available in gray. 05350 is not recommended for electrical insulating applications.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.930 g/cc
0.0336 lb/in³
ASTM D1895
Density 1.74 g/cc
0.0629 lb/in³
ASTM D792
Water Absorption 0.048 %
0.048 %
ASTM D570
Linear Mold Shrinkage 0.0042 cm/cm
0.0042 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 110
110
ASTM D785
Tensile Strength, Ultimate 44.0 MPa
6380 psi
ASTM D638
Elongation at Break 0.32 %
0.32 %
ASTM D638
Tensile Modulus 15.3 GPa
2220 ksi
ASTM D638
Flexural Strength 73.0 MPa
10600 psi
ASTM D790
Flexural Modulus 12.8 GPa
1860 ksi
ASTM D790
Compressive Strength 146 MPa
21200 psi
ASTM D695
Izod Impact, Notched 0.161 J/cm
0.302 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.144 J/cm²
0.685 ft-lb/in²
ASTM D256
Impact 37
37
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 257 °C
495 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 181 °C
358 °F
ASTM D648
Shrinkage 0.086 %
0.086 %
72 hr, 120ºC; ASTM D1299