Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 6401 Phenolic, Briquette, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral/Glass Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 6401 Phenolic, Briquette, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.650 g/cc
0.0235 lb/in³
ASTM D1895
Density 1.73 g/cc
0.0625 lb/in³
ASTM D792
Water Absorption 0.071 %
0.071 %
ASTM D570
Linear Mold Shrinkage 0.0022 cm/cm
0.0022 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 97
97
ASTM D785
Tensile Strength, Ultimate 93.0 MPa
13500 psi
ASTM D638
Elongation at Break 0.73 %
0.73 %
ASTM D638
Tensile Modulus 15.9 GPa
2310 ksi
ASTM D638
Flexural Strength 177 MPa
25700 psi
ASTM D790
Flexural Modulus 14.8 GPa
2150 ksi
ASTM D790
Compressive Strength 251 MPa
36400 psi
ASTM D695
Poissons Ratio 0.33
0.33
ASTM D638
Shear Modulus 5.98 GPa
867 ksi
Calculated
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.390 J/cm²
1.86 ft-lb/in²
ASTM D256
Impact 310
310
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 226 °C
439 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 201 °C
394 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Shrinkage 0.050 %
0.050 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.10e+12 ohm-cm
1.10e+12 ohm-cm
ASTM D247
Dielectric Constant 4.6
4.6
ASTM D150
Dielectric Strength 15.0 kV/mm
381 kV/in
Short Time; ASTM D149
Dissipation Factor 0.286
0.286
ASTM D150
Arc Resistance 70 sec
70 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638