Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 6554 Phenolic, Granular, Compression Molded  (discontinued **)

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Flock Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 6554 Phenolic, Granular, Compression Molded  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-Stage Phenolic. PLENCO 06554 is an organic reinforced phenolic molding compound modified with PTFE to offer improved coefficient of friction values. 06554 is available in black.Information supplied by Plenco
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Apparent Bulk Density 0.580 g/cc
0.0210 lb/in³
Apparent density per ASTM D1895
Water Absorption 0.45 %
0.45 %
ASTM D570
Linear Mold Shrinkage 0.0044 cm/cm
0.0044 in/in
per ATM D955. Post shrinkage is 0.14% at 72hr 120ºC per ASTM D1299.
Mechanical Properties Metric English Comments
Hardness, Rockwell E 75
75
ASTM D785
Tensile Strength, Ultimate 55.7 MPa
8080 psi
ASTM D638
Elongation at Break 0.89 %
0.89 %
ASTM D638
Tensile Modulus 8.27 GPa
1200 ksi
ASTM D638
Flexural Yield Strength 83.2 MPa
12100 psi
ASTM D790
Flexural Modulus 7.72 GPa
1120 ksi
ASTM D790
Compressive Yield Strength 155.3 MPa
22520 psi
ASTM D695
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.220 J/cm²
1.05 ft-lb/in²
ASTM D256
Impact 150
150
J/m Plenco drop ball test
Thermal Properties Metric English Comments
CTE, linear 99.0 µm/m-°C

@Temperature 20.0 °C
55.0 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.370 W/m-K

@Temperature 100 °C
2.57 BTU-in/hr-ft²-°F

@Temperature 212 °F
Maximum Service Temperature, Air 190 °C
374 °F
Heat resistance per ASTM D794
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Electrical Resistivity 2.128e+12 ohm-cm
2.128e+12 ohm-cm
ASTM D257
Dielectric Constant 4.5

@Frequency 1e+6 Hz
4.5

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 16.2 kV/mm
411 kV/in
Short Time; ASTM D149
Dissipation Factor 0.040

@Frequency 1e+6 Hz
0.040

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 60 sec
60 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638