Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 6582 Phenolic, Briquette, Injection Molded

Category Polymer , Thermoset , Phenolic , Phenolic/Rubber; Molded
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 6582 Phenolic, Briquette, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 06582 is a rubber modified phenolic molding compound, offering excellent heat resistant properties, along with improved mechanical strength at elevated temperatures. UL recognized under component file E40654. 06582 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.670 g/cc
0.0242 lb/in³
ASTM D1895
Density 1.59 g/cc
0.0574 lb/in³
ASTM D792
Water Absorption 0.165 %
0.165 %
ASTM D570
Linear Mold Shrinkage 0.00233 cm/cm
0.00233 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 43
43
ASTM D785
Tensile Strength, Ultimate 56.0 MPa
8120 psi
ASTM D638
Elongation at Break 0.75 %
0.75 %
ASTM D638
Tensile Modulus 9.60 GPa
1390 ksi
ASTM D638
Flexural Strength 90.0 MPa
13100 psi
ASTM D790
Flexural Modulus 8.40 GPa
1220 ksi
ASTM D790
Compressive Strength 116 MPa
16800 psi
ASTM D695
Izod Impact, Notched 0.390 J/cm
0.731 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.340 J/cm²
1.62 ft-lb/in²
ASTM D256
Impact 292
292
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 53.0 µm/m-°C

@Temperature 40.0 - 130 °C
29.4 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.440 W/m-K

@Temperature 100 °C
3.05 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 244 °C
471 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 232 °C
450 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 6.00 mm
V-0

@Thickness 0.236 in
Oxygen Index 36 %
36 %
ASTM D2863
Shrinkage 0.128 %
0.128 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 6.40e+11 ohm-cm
6.40e+11 ohm-cm
ASTM D247
Dielectric Constant 5.5
5.5
ASTM D150
Dielectric Strength 10.5 kV/mm
267 kV/in
Step by Step; ASTM D149
12.9 kV/mm
328 kV/in
Short Time; ASTM D149
Dissipation Factor 0.083
0.083
ASTM D150
Arc Resistance 135 sec
135 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638
Users viewing this material also viewed the following: