Material Notes:
PLENCO 06582 is a rubber modified phenolic molding compound, offering excellent heat resistant properties, along with improved mechanical strength at elevated temperatures. UL recognized under component file E40654. 06582 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.660 g/cc
0.0238 lb/in³
ASTM D1895
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Water Absorption 0.155 %
0.155 %
ASTM D570
Linear Mold Shrinkage 0.0011 cm/cm
0.0011 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 44
44
ASTM D785
Tensile Strength, Ultimate 74.0 MPa
10700 psi
ASTM D638
Elongation at Break 0.73 %
0.73 %
ASTM D638
Tensile Modulus 9.20 GPa
1330 ksi
ASTM D638
Flexural Strength 115 MPa
16700 psi
ASTM D790
Flexural Modulus 8.90 GPa
1290 ksi
ASTM D790
Compressive Strength 157 MPa
22800 psi
ASTM D695
Izod Impact, Notched 0.470 J/cm
0.881 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ASTM D256
Impact 276
276
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 230 °C
446 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 241 °C
466 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 6.00 mm
V-0

@Thickness 0.236 in
Oxygen Index 37 %
37 %
ASTM D2863
Shrinkage 0.070 %
0.070 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 6.20e+11 ohm-cm
6.20e+11 ohm-cm
ASTM D247
Dielectric Constant 5.8
5.8
ASTM D150
Dielectric Strength 13.2 kV/mm
335 kV/in
Short Time; ASTM D149
Dissipation Factor 0.077
0.077
ASTM D150
Arc Resistance 120 sec
120 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638