Plenco 6990 Phenolic, Briquette, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral/Glass Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 6990 Phenolic, Briquette, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.770 g/cc
0.0278 lb/in³
ASTM D1895
Density 1.78 g/cc
0.0643 lb/in³
ASTM D792
Water Absorption 0.057 %
0.057 %
ASTM D570
Linear Mold Shrinkage 0.0022 cm/cm
0.0022 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 87
87
ASTM D785
Tensile Strength, Ultimate 56.0 MPa
8120 psi
ASTM D638
Elongation at Break 0.37 %
0.37 %
ASTM D638
Tensile Modulus 17.1 GPa
2480 ksi
ASTM D638
Flexural Strength 123 MPa
17800 psi
ASTM D790
Flexural Modulus 16.3 GPa
2360 ksi
ASTM D790
Compressive Strength 195 MPa
28300 psi
ASTM D695
Izod Impact, Notched 0.370 J/cm
0.693 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.370 J/cm²
1.76 ft-lb/in²
ASTM D256
Impact 164
164
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Thermal Conductivity 0.580 W/m-K

@Temperature 100 °C
4.03 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 241 °C
466 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 0.500 mm
V-0

@Thickness 0.0197 in
Oxygen Index 53 %
53 %
ASTM D2863
Shrinkage 0.0282 %
0.0282 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.20e+12 ohm-cm
1.20e+12 ohm-cm
ASTM D247
Dielectric Constant 5.6
5.6
ASTM D150
Dielectric Strength 11.6 kV/mm
295 kV/in
Short Time; ASTM D149
Dissipation Factor 0.048
0.048
ASTM D150
Arc Resistance 185 sec
185 sec
ASTM D495
Comparative Tracking Index 250 V
250 V
ASTM D3638