Plenco 7300 Phenolic, Nodular, Injection Molded  (discontinued **)

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 7300 Phenolic, Nodular, Injection Molded  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-Stage Phenolic. PLENCO 07300 is an organic fiber reinforced phenolic molding compound offering improved mechanical strength and excellent cosmetic properties. UL recognized under component file E40654. 07300 is available in black.Information supplied by Plenco
Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
Apparent Bulk Density 0.630 g/cc
0.0228 lb/in³
Apparent density per ASTM D1895
Water Absorption 0.25 %
0.25 %
ASTM D570
Linear Mold Shrinkage 0.0075 cm/cm
0.0075 in/in
per ATM D955. Post shrinkage is 0.4% at 72hr 120ºC per ASTM D1299.
Mechanical Properties Metric English Comments
Hardness, Rockwell E 90
90
ASTM D785
Tensile Strength, Ultimate 61.8 MPa
8960 psi
ASTM D638
Elongation at Break 1.32 %
1.32 %
ASTM D638
Tensile Modulus 8.97 GPa
1300 ksi
ASTM D638
Flexural Yield Strength 87.1 MPa
12600 psi
ASTM D790
Flexural Modulus 7.38 GPa
1070 ksi
ASTM D790
Compressive Yield Strength 210.6 MPa
30550 psi
ASTM D695
Charpy Impact, Notched 0.210 J/cm²
0.999 ft-lb/in²
ASTM D256
Impact 122
122
J/m Plenco drop ball test
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 198 °C
388 °F
Heat resistance per ASTM D794
Deflection Temperature at 1.8 MPa (264 psi) 161 °C
322 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.71e+11 ohm-cm
1.71e+11 ohm-cm
ASTM D257
Dielectric Constant 5.0

@Frequency 1e+6 Hz
5.0

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 12.6 kV/mm
320 kV/in
Short Time; ASTM D149
Dissipation Factor 0.045

@Frequency 1e+6 Hz
0.045

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 100 sec
100 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638