Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral/Flock Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 7466 Phenolic, Granular, Transfer Molded  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-Stage Phenolic. PLENCO 07466 is a flock cotton and mineral filled phenolic molding compound offering excellent heat resistance and dimensional stability. UL recognized under component file E40654. 07466 is available in black.Information supplied by Plenco
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ASTM D792
Apparent Bulk Density 0.620 g/cc
0.0224 lb/in³
Apparent density per ASTM D1895
Water Absorption 0.11 %
0.11 %
ASTM D570
Linear Mold Shrinkage 0.0043 cm/cm
0.0043 in/in
ATM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 86
86
ASTM D785
Tensile Strength, Ultimate 58.1 MPa
8430 psi
ASTM D638
Elongation at Break 0.84 %
0.84 %
ASTM D638
Tensile Modulus 8.61 GPa
1250 ksi
ASTM D638
Flexural Yield Strength 88.7 MPa
12900 psi
ASTM D790
Flexural Modulus 9.47 GPa
1370 ksi
ASTM D790
Compressive Yield Strength 203 MPa
29400 psi
ASTM D695
Izod Impact, Notched 0.240 J/cm
0.450 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.220 J/cm²
1.05 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 205 °C
401 °F
Heat resistance per ASTM D794
Deflection Temperature at 1.8 MPa (264 psi) 193 °C
379 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.47 mm
V-0

@Thickness 0.0579 in
Electrical Properties Metric English Comments
Electrical Resistivity 2.00e+11 ohm-cm
2.00e+11 ohm-cm
ASTM D257
Dielectric Constant 5.8

@Frequency 1e+6 Hz
5.8

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 11.9 kV/mm
302 kV/in
Short Time; ASTM D149
Dissipation Factor 0.061

@Frequency 1e+6 Hz
0.061

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 180 sec
180 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638