Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 7507 Phenolic, Granular, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Resole, Wood Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 7507 Phenolic, Granular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solutions at elevated temperature. UL recognized under component file E40654. 07507 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.620 g/cc
0.0224 lb/in³
ASTM D1895
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
Water Absorption 0.44 %
0.44 %
ASTM D570
Linear Mold Shrinkage 0.0063 cm/cm
0.0063 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 57
57
ASTM D785
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Elongation at Break 1.12 %
1.12 %
ASTM D638
Tensile Modulus 7.90 GPa
1150 ksi
ASTM D638
Flexural Strength 76.0 MPa
11000 psi
ASTM D790
Flexural Modulus 7.20 GPa
1040 ksi
ASTM D790
Compressive Strength 157 MPa
22800 psi
ASTM D695
Poissons Ratio 0.33
0.33
ASTM D638
Shear Modulus 2.97 GPa
431 ksi
Calculated
Izod Impact, Notched 0.179 J/cm
0.335 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.196 J/cm²
0.933 ft-lb/in²
ASTM D256
Impact 125
125
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 37.0 µm/m-°C

@Temperature 40.0 - 130 °C
20.6 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.460 W/m-K

@Temperature 100 °C
3.19 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 204 °C
399 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 186 °C
367 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
Oxygen Index 31 %
31 %
ASTM D2863
Shrinkage 0.42 %
0.42 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 8.30e+11 ohm-cm
8.30e+11 ohm-cm
ASTM D247
Dielectric Constant 7.0
7.0
ASTM D150
Dielectric Strength 8.00 kV/mm
203 kV/in
Short Time; ASTM D149
Dissipation Factor 0.172
0.172
ASTM D150
Arc Resistance 177 sec
177 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638
Copyright © lookpolymers.com All Rights Reserved