Plenco 7507 Phenolic, Granular, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Resole, Wood Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 7507 Phenolic, Granular, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solutions at elevated temperature. UL recognized under component file E40654. 07507 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.610 g/cc
0.0220 lb/in³
ASTM D1895
Density 1.53 g/cc
0.0553 lb/in³
ASTM D792
Water Absorption 0.37 %
0.37 %
ASTM D570
Linear Mold Shrinkage 0.00233 cm/cm
0.00233 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 75
75
ASTM D785
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Tensile Modulus 8.00 GPa
1160 ksi
ASTM D638
Flexural Strength 90.0 MPa
13100 psi
ASTM D790
Flexural Modulus 8.60 GPa
1250 ksi
ASTM D790
Compressive Strength 179 MPa
26000 psi
ASTM D695
Izod Impact, Notched 0.209 J/cm
0.392 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.220 J/cm²
1.05 ft-lb/in²
ASTM D256
Impact 125
125
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 203 °C
397 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 225 °C
437 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
Shrinkage 0.28 %
0.28 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.70e+12 ohm-cm
1.70e+12 ohm-cm
ASTM D247
Dielectric Constant 6.4
6.4
ASTM D150
Dielectric Strength 10.9 kV/mm
277 kV/in
Short Time; ASTM D149
Dissipation Factor 0.070
0.070
ASTM D150
Arc Resistance 179 sec
179 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638