Material Notes:
This Valite product has been replaced by Plenco 4100. Data provided by Plenco.VALITE 4100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability characteristics and molded finish. It is used in applicance and oil field applications and can be molded by compression, transfer, or injection processes. It is UL recognized under component file E59891. VALITE 4100 is the same formulation as PLENCO 04100. Plenco drop ball 113g test value is 26 cm.Plenco has discontinued their Valite product line.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ASTM D792
Apparent Bulk Density 0.740 g/cc
0.0267 lb/in³
ASTM D1895
Water Absorption 0.26 %
0.26 %
ASTM D570
Linear Mold Shrinkage 0.0081 cm/cm
0.0081 in/in
Post shrinkage is 0.27% at 72hr 120°C.; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 80
80
ASTM D785
Tensile Strength, Ultimate 56.8 MPa
8240 psi
ASTM D638
Elongation at Break 0.90 %
0.90 %
ASTM D638
Tensile Modulus 9.20 GPa
1330 ksi
ASTM D638
Flexural Yield Strength 88.1 MPa
12800 psi
ASTM D790
Flexural Modulus 8.20 GPa
1190 ksi
ASTM D790
Compressive Yield Strength 189.9 MPa
27540 psi
ASTM D695
Charpy Impact, Notched 0.170 J/cm²
0.809 ft-lb/in²
J/cm; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 199 °C
390 °F
Heat Resistance; ASTM D795
Deflection Temperature at 1.8 MPa (264 psi) 176 °C
349 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.47 mm
V-1

@Thickness 0.0579 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.15e+11 ohm-cm
1.15e+11 ohm-cm
ASTM D257
Dielectric Constant 5.2

@Frequency 1e+6 Hz
5.2

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 7.40 kV/mm
188 kV/in
Step-by-Step; ASTM D149
10.5 kV/mm
267 kV/in
Short Term per ASTM D149
Dissipation Factor 0.067

@Frequency 1e+6 Hz
0.067

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 150 sec
150 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638