Plenco Valite 697-A Novolac Phenolic, Granular, Compression Molded  (discontinued **)

Category Polymer , Thermoset , Phenolic , Phenolic, Novolac, Impact Grade, Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco Valite 697-A Novolac Phenolic, Granular, Compression Molded  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This Valite product has been replaced by Plenco 7697. Data provided by Plenco.VALITE 697-A is a black, two stage, improved impact phenolic molding compound. It has been specifically formulated for automotive pulleys. It is used in automotive and oil well applications anc can be molded by compression, transfer, or injection precesses. VALITE 697-A is the same formulation as PLENCO 07697. Plenco drop ball 113g test value is 55 cm.Plenco has discontinued their Valite product line.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
ASTM D792
Apparent Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
Water Absorption 0.30 %
0.30 %
ASTM D570
Linear Mold Shrinkage 0.0035 cm/cm
0.0035 in/in
Post shrinkage is 0.17% at 72hr 120°C.; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 90
90
ASTM D785
Tensile Strength, Ultimate 60.3 MPa
8750 psi
ASTM D638
Elongation at Break 0.70 %
0.70 %
ASTM D638
Tensile Modulus 10.0 GPa
1450 ksi
ASTM D638
Flexural Yield Strength 92.2 MPa
13400 psi
ASTM D790
Flexural Modulus 9.10 GPa
1320 ksi
ASTM D790
Compressive Yield Strength 227.3 MPa
32970 psi
ASTM D695
Izod Impact, Notched 0.250 J/cm
0.468 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.280 J/cm²
1.33 ft-lb/in²
J/cm; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 199 °C
390 °F
Heat Resistance; ASTM D795
Deflection Temperature at 1.8 MPa (264 psi) 206 °C
403 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 4.09e+12 ohm-cm
4.09e+12 ohm-cm
ASTM D257
Dielectric Constant 4.5

@Frequency 1e+6 Hz
4.5

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm
381 kV/in
Short Term per ASTM D149.
Dissipation Factor 0.036

@Frequency 1e+6 Hz
0.036

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 140 sec
140 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638