Material Notes:
POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal graphite to each application. Post synthesis modifications enhance the original material to allow even greater flexibility for highly specialized conditions.
Physical Properties Metric English Comments
Apparent Bulk Density 1.77 g/cc
0.0639 lb/in³
Open Porosity 75 %
75 %
Porosity 21 %
21 %
Particle Size 5.0 µm
5.0 µm
Pore Size 0.800 microns
0.0315 mil
Mechanical Properties Metric English Comments
Hardness, Shore D 95
95
Tensile Strength, Yield 69.0 MPa
10000 psi
Elongation at Yield 0.62 %
0.62 %
Modulus of Elasticity 11.0 GPa
1600 ksi
Flexural Strength 97.0 MPa
14100 psi
Compressive Strength 186 MPa
27000 psi
Thermal Properties Metric English Comments
CTE, linear 7.60 µm/m-°C
4.22 µin/in-°F
Thermal Conductivity 60.0 W/m-K
416 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00246 ohm-cm
0.00246 ohm-cm