Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Poco Graphite PLS Semiconductor Grade Graphite

Category Carbon , Graphite
Manufacturer Poco Graphite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Poco Graphite PLS Semiconductor Grade Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their performance under specific conditions. The manufacturing process for each grade is tightly controlled to produce materials that have a uniform microstructure and the right balance of strength, grain size and hardness to offer optimum performance for their intended applications.
Physical Properties Metric English Comments
Apparent Bulk Density 1.82 g/cc
0.0658 lb/in³
Particle Size 10 µm
10 µm
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
Tensile Strength, Yield 40.0 MPa
5800 psi
Estimated at 70% of flexural strength
Flexural Strength 60.0 MPa
8700 psi
Compressive Strength 110 MPa
16000 psi
Thermal Properties Metric English Comments
CTE, linear 8.30 µm/m-°C
4.61 µin/in-°F
Thermal Conductivity 105 W/m-K
729 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00122 ohm-cm
0.00122 ohm-cm
Descriptive Properties Value Comments
Oxidation Threshold 460°C
Temperature that results in 1% weight loss in 24 hours. Oxidation threshold increases by approximately 100°C if graphite is purified.
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved