Polikim ULPOLEN® 1000 UHMWPE, Flame Retardant

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Polikim Polimer ve Kimya Sanay
Trade Name ULPOLEN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polikim ULPOLEN® 1000 UHMWPE, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For those producing flammable materials and in the mining industry, explosion and fire are major dangers. It is of vital importance that in conveyor belts and bunkers, lining material is flame retardant. It is possible to improve Ulpolen ® 1000's technical properties through additives depending on the application. Additives inevitibly increase cost, but when life time of material and initial lining effort are considered, advantages of selecting the right material become evident. Flame retardant Ulpolen ® 1000 does not contain halogen and antimony. Smoke absorption is minimum.Information provided by Polikim Polimer.
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ISO 1183
Water Absorption at Saturation <= 0.010 %
<= 0.010 %
DIN 53495
Molecular Weight 9.20e+6 g/mol
9.20e+6 g/mol
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ISO 868
Tensile Strength, Ultimate 22.0 MPa
3190 psi
ISO 527-1
Elongation at Break >= 350 %
>= 350 %
ISO 527-1
Tensile Modulus 0.800 GPa
116 ksi
ISO 527-1
Izod Impact, Notched (ISO) 100 kJ/m²
47.6 ft-lb/in²
15°V; ISO 179
Coefficient of Friction 0.10 - 0.15
0.10 - 0.15
Sand Slurry 100
100
Thermal Properties Metric English Comments
CTE, linear 200 µm/m-°C

@Temperature 20.0 - 100 °C
111 µin/in-°F

@Temperature 68.0 - 212 °F
DIN 53752
Thermal Conductivity 0.400 W/m-K
2.77 BTU-in/hr-ft²-°F
DIN 52612
Melting Point 135 °C
275 °F
Maximum Service Temperature, Air 80.0 °C
176 °F
continuous
130 °C
266 °F
short term
Minimum Service Temperature, Air -250 °C
-418 °F
-250 °C
-418 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1000 ohm-cm
1000 ohm-cm
DIN VDE 0303
Surface Resistance 10000 ohm
10000 ohm
DIN VDE 0303
Arc Resistance 180 - 240 sec
180 - 240 sec
DIN VDE 0303