Polimeri Europa EDISTIR PD RK4122H High Impact Polystyrene (HIPS)  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa EDISTIR PD RK4122H High Impact Polystyrene (HIPS)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,078-06-04-23 UL94 V-2, halogen and antimony free, medium impact polystyrene. This grade features enhanced thermal stability in the injection molding process and good mechanical properties. Applications: Examples of applications are TV back covers, printers and copiers.Unfilled. Suitable for Injection Molding. Supplied as pellets. Contains release agent.ISO data. Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
Melt Flow 6.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
cm³/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.0 MPa
4930 psi
50 mm/min
Elongation at Break 30 %
30 %
Nominal
Tensile Modulus 2.45 GPa
355 ksi
1 mm/min
Charpy Impact Unnotched 8.50 J/cm²
40.5 ft-lb/in²
7.00 J/cm²

@Temperature -30.0 °C
33.3 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
0.400 J/cm²

@Temperature -30.0 °C
1.90 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Vicat Softening Point 80.0 °C
176 °F
50°C/hr; 50N
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
Dielectric Constant 2.5

@Frequency 100 Hz
2.5

@Frequency 100 Hz
Dielectric Strength 65.0 kV/mm
1650 kV/in
Dissipation Factor 0.00060

@Frequency 100 Hz
0.00060

@Frequency 100 Hz
Comparative Tracking Index 475 V
475 V
Users viewing this material also viewed the following: