Polimeri Europa EDISTIR PD RK5512G High Impact Polystyrene (HIPS)  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa EDISTIR PD RK5512G High Impact Polystyrene (HIPS)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,088-06-07-23 UL94 V-2, polybromobiphenylether (PBBE) free, high impact polystyrene with good mechanical and thermal properties. It exhibits a good stability to the processing conditions and the light exposure. This grade is recommended for injection molding in the electronic industry. Applications: TV back covers, computer housings, printers and copiers.Unfilled. Suitable for Injection Molding. Supplied as pellets. Contains release agent. Contains release agent.ISO data. Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
Melt Flow 5.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
cm³/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.0 MPa
3340 psi
50 mm/min
Elongation at Break 50 %
50 %
Nominal
Elongation at Yield 2.0 %
2.0 %
50 mm/min
Tensile Modulus 2.10 GPa
305 ksi
1 mm/min
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 0.750 J/cm²
3.57 ft-lb/in²
0.400 J/cm²

@Temperature -30.0 °C
1.90 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Vicat Softening Point 90.0 °C
194 °F
50°C/hr; 50N
Flammability, UL94 V-2

@Thickness 1.70 mm
V-2

@Thickness 0.0669 in
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
Dielectric Constant 2.5

@Frequency 100 Hz
2.5

@Frequency 100 Hz
Dielectric Strength 65.0 kV/mm
1650 kV/in
Dissipation Factor 0.00060

@Frequency 100 Hz
0.00060

@Frequency 100 Hz
Comparative Tracking Index 475 V
475 V