Polimeri Europa EDISTIR RK0414 High Impact Polystyrene (HIPS)  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa EDISTIR RK0414 High Impact Polystyrene (HIPS)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,088-03-04-23 UL94 V-0, polybromobiphenylether (PBBE) free, flame retarded high impact polystyrene with excellent light stability. This grade combines medium flow and heat resistance for injection molding of technical parts. Applications: Computer housings, fan and ventilators, printers, copiers and electrical appliances.Unfilled. Suitable for Injection Molding. Supplied as pellets. Contains release agent.ISO data. Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
Melt Flow 4.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
4.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
cm³/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.0 MPa
4210 psi
50 mm/min
Elongation at Break 40 %
40 %
Nominal
Elongation at Yield 1.5 %
1.5 %
50 mm/min
Tensile Modulus 2.20 GPa
319 ksi
1 mm/min
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
5.50 J/cm²

@Temperature -30.0 °C
26.2 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
0.350 J/cm²

@Temperature -30.0 °C
1.67 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °C
169 °F
Vicat Softening Point 90.0 °C
194 °F
50°C/hr; 50N
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
Dielectric Constant 2.5

@Frequency 100 Hz
2.5

@Frequency 100 Hz
Dielectric Strength 65.0 kV/mm
1650 kV/in
Dissipation Factor 0.00040

@Frequency 100 Hz
0.00040

@Frequency 100 Hz
Comparative Tracking Index 400 V
400 V