Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Eraclene® MM 74 High Density Polyethylene - Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Eraclene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Eraclene® MM 74 High Density Polyethylene - Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Eraclene MM 74 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 74 is characterized by a good balance between rigidity and impact resistance. The resin is UV stabilized and is recommended for the production of items for outdoor exposure.Main Applications: Eraclene MM 74 is specifically designed for pails, lids for light-weight containers, agricultural containers, houseware and dust bins.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.953 g/cc
0.953 g/cc
ISO 1183
Melt Flow 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
12 g/10 min

@Load 5.00 kg,
Temperature 190 °C
12 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ISO 868/A
Tensile Strength at Break 19.0 MPa
2760 psi
ISO 527
Tensile Strength, Yield 26.0 MPa
3770 psi
ISO 527
Elongation at Break 600 %
600 %
ISO 527
Flexural Modulus 1.20 GPa
174 ksi
ISO 178
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ISO 180/A
Thermal Properties Metric English Comments
Melting Point 134 °C
273 °F
Internal method
Vicat Softening Point 126 °C

@Load 1.00 kg
259 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746