Polimeri Europa Eraclene® MQ 74 High Density Polyethylene - Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Eraclene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Eraclene® MQ 74 High Density Polyethylene - Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Eraclene MQ 74 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application. This resin is suggested in applications for which high creep, impact and stress cracking resistance are required.Eraclene MQ 74 is UV stabilized and is recommended for the production of items for outdoor exposure.Main Applications: Eraclene MQ 74 is suggested to produce items with good mechanical properties: Light-weight crates, houseware. For its flowability, the resin can be used whenever high production rate is required.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.952 g/cc
0.952 g/cc
ISO 1183
Melt Flow 11 g/10 min

@Load 2.16 kg,
Temperature 190 °C
11 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ISO 868/A
Tensile Strength at Break 15.0 MPa
2180 psi
ISO 527
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO 527
Elongation at Break 300 %
300 %
ISO 527
Flexural Modulus 1.25 GPa
181 ksi
ISO 178
Izod Impact, Notched 0.650 J/cm
1.22 ft-lb/in
ISO 180/A
Thermal Properties Metric English Comments
Melting Point 134 °C
273 °F
Internal method
Vicat Softening Point 125 °C

@Load 1.00 kg
257 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746