Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Eraclene® PF 92 High Density Polyethylene - Pipe Grade Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Eraclene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Eraclene® PF 92 High Density Polyethylene - Pipe Grade Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Eraclene PF 92 is a homopolymer high density polyethylene resin (HDPE) with antioxidants, suitable for pipe application. It is characterized by high rigidity, high impact strength and low swelling.Eraclene PF 92 has an intermediate molecular weight distribution which perfectly balances overall performances with ease of processing.Main Applications: Eraclene PF 92 is recommended for the production of structured wall pipes when high rigidity is required. It can be used for the production of sheets and profiles.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ISO 1183
Melt Flow 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
2.6 g/10 min

@Load 5.00 kg,
Temperature 190 °C
2.6 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
45 g/10 min

@Load 21.6 kg,
Temperature 190 °C
45 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ISO 868/A
Tensile Strength at Break 30.0 MPa
4350 psi
ISO 527
Tensile Strength, Yield 31.0 MPa
4500 psi
ISO 527
Elongation at Break >= 800 %
>= 800 %
ISO 527
Flexural Modulus 1.50 GPa
218 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 138 °C
280 °F
Internal method
Vicat Softening Point 128 °C

@Load 1.00 kg
262 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746
Users viewing this material also viewed the following: