Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Europrene® SOL B 183 Styrene - Butadiene Copolymer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Europrene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Europrene® SOL B 183 Styrene - Butadiene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Europrene® SOL B 183 is a solution styrene-butadiene partial block copolymer, polymerized using an alkyl lithium catalyst. A non-staining antioxidant is added during the production process.Key Features: The presence of styrene both bound and block at lower than normal concentrations allows Europrene® SOL B 183 to exhibit fast dissolving characteristics and dispersion in the plastic matrix of styrene polymers and copolymers. The higher level of polybutadiene in the copolymer allows for the possibility of higher impact properties.Main Applications: Impact improver of ABS and Polystyrene giving a gloss surface.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Volatiles <= 1.0 %
<= 1.0 %
ASTM D5668
Viscosity 32 cP

@Temperature 25.0 °C
32 cP

@Temperature 77.0 °F
of Solution, 5% wt/wt in Styrene
Mooney Viscosity 65

@Temperature 100 °C
65

@Temperature 212 °F
ASTM D1646
Ash <= 0.10 %
<= 0.10 %
ASTM D5667
Chemical Properties Metric English Comments
Styrene Content 7.0 %
7.0 %
Block; Internal Method
11 %
11 %
Bound; ASTM D5775