Polimeri Europa Europrene® SOL R C2525 Styrene - Butadiene Copolymer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Europrene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Europrene® SOL R C2525 Styrene - Butadiene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Europrene® SOL R C2525 is a solution polymerized dry styrene-butadiene random copolymer. It is produced by continuous polymerization process.Key Features: Europrene® SOL R C2525 is the solution grade alternative to Europrene® 1502; thanks to its controlled microstructure and molecular weight distribution, it exhibits better dimensional stability and compression set behavior in compounds. Its low Tg makes it suitable for low RR tire application.Main Applications: Carbon Black-based compounds for low rolling resistance tire treads, mechanical goods, footwear.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Volatiles <= 0.75 %
<= 0.75 %
ASTM D5668
Mooney Viscosity 54

@Temperature 100 °C
54

@Temperature 212 °F
ASTM D1646
Vinyl Acetate Content 24 %
24 %
Referred to butadiene portion; Internal Method
Ash <= 0.20 %
<= 0.20 %
ASTM D5667
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -51.0 °C
-59.8 °F
Internal Method
Chemical Properties Metric English Comments
Styrene Content 26 %
26 %
Bound; ASTM D5775