Polimeri Europa Europrene® SOL R C2564-T Styrene - Butadiene Copolymer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Europrene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Europrene® SOL R C2564-T Styrene - Butadiene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Europrene® SOL R C2564-T is a solution polymerized, oil extended styrene-butadiene random copolymer. The polymer is extended with a TDAE oil and contains a non-staining antioxidant. It is produced by continuous polymerization process.Key Features: Europrene® SOL R C2564-T has a microstructure, molecular weight distribution and branching designed to yield processability with a good balance of dynamic properties. Europrene® SOL R C2564-T is the TDAE oil extended alternative to Europrene® SOL R 2564-A. the more plastifying capability of TDAE oil extension combines a certain advantage in processability with an hysteretical gain mainly in rolling resistance improvement.Main Applications: Silica black-based compounds for low rolling resistance tire treads with improved wet grip, mechanical goods.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Volatiles <= 0.20 %
<= 0.20 %
ASTM D5668
Mooney Viscosity 50

@Temperature 100 °C
50

@Temperature 212 °F
ASTM D1646
Vinyl Acetate Content 64 %
64 %
Referred to butadiene portion; Internal Method
Ash <= 0.75 %
<= 0.75 %
ASTM D5667
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -26.0 °C
-14.8 °F
Internal Method
Chemical Properties Metric English Comments
Styrene Content 25 %
25 %
Bound; ASTM D5775
Descriptive Properties Value Comments
Oil Content (phr) 37.5
ASTM D5774