Polimeri Europa Europrene® SOL T 172 Styrene - Butadiene Block Copolymer

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Europrene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Europrene® SOL T 172 Styrene - Butadiene Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Europrene® SOL T 172 is a radial block copolymer obtained by anionic polymerization. The polymer is based on styrene and butadiene, where bound styrene is 30% weight. The polymer is extended with paraffinic oil (45 phr). A non-staining antioxidant system is added during the production process.Key Features: Europrene® SOL T 172 is a block copolymer with radial structure, where the oil addition allows extremely good flow characteristics and an easy processability. The grade provides excellent mechanical properties and outstanding abrasion resistance, in a wide range of formulated products.Main Applications: Used as a high strength base in formulated compounds for footwear and technical applications, the grade is used in the modification of polymers and in plastic recycling.Information provided by Polimeri Europa. Mechanical properties measured on ASTM D 4703 compression molded samples.
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 190 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 46
46
ASTM D2240
Tensile Strength at Break 9.00 MPa
1310 psi
ASTM D412
Elongation at Break 900 %
900 %
ASTM D412
300% Modulus 0.00140 GPa
0.203 ksi
ASTM D412
Abrasion 90
90
[mm³]; DIN 53516