Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Europrene® SOL T 177 Styrene - Butadiene Block Copolymer

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Europrene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Europrene® SOL T 177 Styrene - Butadiene Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Europrene® SOL T 177 is a radial block copolymer obtained by anionic polymerization. The polymer is based on styrene and butadiene, where bound styrene is 50% weight. The polymer is extended with paraffinic oil (40 phr). A non-staining antioxidant system is added during the production process.Key Features: Europrene® SOL T 177 is a block copolymer with radial structure, providing excellent mechanical properties, high strength and elasticity in a wide range of formulated products. The oil addition allows good flow characteristics.Main Applications: Used as a high strength base in formulated compounds for footwear, the grade is specifically designed for high hardness compounds.Information provided by Polimeri Europa. Mechanical properties measured on ASTM D 4703 compression molded samples.
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Melt Flow 15 g/10 min

@Load 5.00 kg,
Temperature 190 °C
15 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
ASTM D2240
Tensile Strength at Break 15.0 MPa
2180 psi
ASTM D412
Elongation at Break 950 %
950 %
ASTM D412
300% Modulus 0.00300 GPa
0.435 ksi
ASTM D412
Abrasion 170
170
[mm³]; DIN 53516