Polimeri Europa Europrene® SOL T 6302 Styrene - Butadiene Block Copolymer

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Europrene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Europrene® SOL T 6302 Styrene - Butadiene Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Europrene® SOL T 6302 is a linear block copolymer obtained by anionic polymerization. The polymer is based on styrene and butadiene, where bound styrene is 30% weight. A non-staining antioxidant system is added during the production process.Key Features: Europrene® SOL T 6302 is a linear block copolymer, providing excellent mechanical properties, high strength and elasticity, combined with good dispersability and processability.Main Applications: Used in bitumen modification, particularly in road paving applications, in compounding for both footwear and technical goods, and in adhesive applications.Information provided by Polimeri Europa. Mechanical properties measured on ASTM D 4703 compression molded samples.
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Brookfield Viscosity 0.40 cP
0.40 cP
Toluene sol., 25% wt; ASTM D1084
Melt Flow <= 1.0 g/10 min

@Load 5.00 kg,
Temperature 190 °C
<= 1.0 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength at Break 20.0 MPa
2900 psi
ASTM D412
Elongation at Break 750 %
750 %
ASTM D412
300% Modulus 0.00250 GPa
0.363 ksi
ASTM D412