Polimeri Europa Europrene® SOL TH 2312 Styrene - Ethylene / Butylene Block Copolymer

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Europrene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Europrene® SOL TH 2312 Styrene - Ethylene / Butylene Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Europrene® SOL TH 2312 is a linear block copolymer obtained by selective hydrogenation of styrene-butadiene-styrene block copolymers. The polymer is based on styrene and ethylene/butylene, where bound styrene content is 30%wt. A non-staining, TNPP free antioxidant system is added during the production process.Key Features: Europrene® SOL TH 2312 is a linear triblock copolymer of medium molecular weight. It is characterized by excellent processability, mechanical properties and ageing resistance.Main Applications: Europrene® SOL TH 2312 is designed for hot melt adhesives and polymer modification. The grade is also widely used in technical compounds where softness and clarity are required. Due to its easy dispersibility, SOL TH 2312 can be used in bitumen modification for roofing applications.Information provided by Polimeri Europa. Mechanical properties measured on ASTM D 4703 compression molded samples.
Physical Properties Metric English Comments
Brookfield Viscosity 0.16 cP
0.16 cP
Toluene sol., 20% wt; ASTM D1084
Melt Flow <= 1.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
<= 1.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ASTM D2240
Tensile Strength at Break 30.0 MPa
4350 psi
ASTM D412
Elongation at Break 600 %
600 %
ASTM D412
300% Modulus 0.00500 GPa
0.725 ksi
ASTM D412