Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Extir® Verdi VR A3000 AE Expandable Polystyrene - Flame Retardant

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Extir®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Extir® Verdi VR A3000 AE Expandable Polystyrene - Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description:Extir Verdi VR A3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain CFC or HCFC.Extir VR A3000 AE is an improvement of A 3000 AE showing an improved thermal conductivity.Extir A3000 AE is used for production of shaped moldings with section greater than 8 mm and of medium-high density blocks.Applications: Extir Verdi VR 3000 AE has an improved thermal conductivity value, especially at low density. Extir VR A3000 AE is used mainly in building and industrial packaging applications where, for legislative or safety reasons, the use of flame retardant material is required.Typical applications areindustrial packaging, e.g. cathode ray tube protectionmedium-high density blocks for thermal insulationwindow dressing, theatre backgroundsmolded panels for underfloor heatingmolded or block-cut building componentsInformation provided by Polimeri Europa.
Physical Properties Metric English Comments
Bulk Density 0.590 - 0.630 g/cc
0.0213 - 0.0228 lb/in³
Density >= 0.0160 g/cc
>= 0.000578 lb/in³
Minimum apparent density on a discontinuous pre-expander
>= 0.0170 g/cc
>= 0.000614 lb/in³
Minimum apparent density on a continuous pre-expander after one expansion
0.0160 - 0.0300 g/cc
0.000578 - 0.00108 lb/in³
Density range normally used
Particle Size 600 - 1000 µm
600 - 1000 µm
Users viewing this material also viewed the following: