Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Extir® Verdi VR A5000 AE Expandable Polystyrene - Flame Retardant

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Extir®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Extir® Verdi VR A5000 AE Expandable Polystyrene - Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
b>Product Description:Extir Verdi VR A5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent.Extir does not contain CFC or HCFC.Extir VR A5000 AE is an improvement of A 5000 AE showing an improved thermal conductivity.Extir A5000 AE is used for production of low-medium density blocks for the thermal insulation sector.Applications: Extir Verdi VR A5000 AE has an improved thermal conductivity value, especially at low density. Extir VR A5000 AE is used mainly in the construction sector where, for legislative or safety reasons, the use of flame retardant material is required.Typical applications areblocks, especially for external thermal insulationlow density elasticized blocks for impact sound absorption (Trittschall)void formers, trough formers and culvert formers cut from blockblocks or slabs for road foundations and civil constructionInformation provided by Polimeri Europa.
Physical Properties Metric English Comments
Bulk Density 0.590 - 0.630 g/cc
0.0213 - 0.0228 lb/in³
Density >= 0.0100 g/cc
>= 0.000361 lb/in³
Minimum apparent density on a continuous pre-expander after two expansions
>= 0.0150 g/cc
>= 0.000542 lb/in³
Minimum apparent density on a continuous pre-expander after one expansion
0.0110 - 0.0200 g/cc
0.000397 - 0.000723 lb/in³
Density range normally used
>= 0.0160 g/cc
>= 0.000578 lb/in³
Minimum apparent density on a discontinuous pre-expander
Particle Size 900 - 1600 µm
900 - 1600 µm