Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Flexirene® FG 20 U Butene Copolymer Linear Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Butene, Film
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Flexirene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Flexirene® FG 20 U Butene Copolymer Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flexirene FG 20 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 U is recommended for the production of general purpose film, in blend or coextrusion with LDPE.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.918 g/cc
0.918 g/cc
ISO 1183
Thickness 15.0 - 50.0 microns
0.591 - 1.97 mil
Recommended
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 10.0 MPa
1450 psi
ISO 527-3
Film Tensile Strength at Yield, TD 10.0 MPa
1450 psi
ISO 527-3
Film Elongation at Break, MD 600 %
600 %
ISO 527-3
Film Elongation at Break, TD 750 %
750 %
ISO 527-3
Coefficient of Friction, Dynamic >= 0.50
>= 0.50
ISO 8295
Elmendorf Tear Strength, MD 2.5475 g/micron
64.706 g/mil
ISO 6383-2
Elmendorf Tear Strength, TD 17.323 g/micron
440.00 g/mil
ISO 6383-2
Dart Drop Test 120 g
0.265 lb
F50; ISO 7765-1
Film Tensile Strength at Break, MD 42.0 MPa
6090 psi
ISO 527-3
Film Tensile Strength at Break, TD 33.0 MPa
4790 psi
ISO 527-3
1% Secant Modulus, MD 150 MPa
21800 psi
ISO 527-3
1% Secant Modulus, TD 175 MPa
25400 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 123 °C
253 °F
Internal method
Vicat Softening Point 100 °C

@Load 1.00 kg
212 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Optical Properties Metric English Comments
Haze 10 %
10 %
ISO 14782
Gloss 60 %
60 %
45°; ASTM D2457