Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Greenflex® ML 40 Ethylene Vinyl Acetate Copolymer - Injection Molding

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate; Molded/Extruded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Greenflex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Greenflex® ML 40 Ethylene Vinyl Acetate Copolymer - Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Greenflex ML 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding of flexible items. Items produced with Greenflex ML 40 show high elasticity and flexibility.Main Applications: Greenflex ML 40 is recommended for the production of flexible items.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.935 g/cc
0.935 g/cc
ISO 1183
Vinyl Acetate Content 14 %
14 %
Internal Method
Melt Flow 2.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 92
92
ISO 868/A
Hardness, Shore D 40
40
ISO 868/A
Tensile Strength, Yield 6.00 MPa
870 psi
ISO 527
Flexural Modulus 0.0600 GPa
8.70 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 91.0 °C
196 °F
Internal Method
Vicat Softening Point 63.0 °C

@Load 1.00 kg
145 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746
Users viewing this material also viewed the following: