Polimeri Europa Greenflex® MP 34 Ethylene Vinyl Acetate Copolymer - Injection Molding & Compounding

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate; Molded/Extruded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Greenflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Greenflex® MP 34 Ethylene Vinyl Acetate Copolymer - Injection Molding & Compounding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Greenflex MP 34 is an ethylene vinyl acetate copolymer (EVA) for injection molding and compounding applications. Greenflex MP 34 combines high fluidity with high elasticity.Main Applications: Greenflex MP 34 is recommended for the production of articles with a high degree of elasticity, such as gaskets and foamed caps for wine.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.929 g/cc
0.929 g/cc
ISO 1183
Vinyl Acetate Content 9.0 %
9.0 %
Internal Method
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ISO 868/A
Hardness, Shore D 40
40
ISO 868/A
Tensile Strength, Yield 7.00 MPa
1020 psi
ISO 527
Flexural Modulus 0.0900 GPa
13.1 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 95.0 °C
203 °F
Internal Method
Vicat Softening Point 70.0 °C

@Load 1.00 kg
158 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746