Polimeri Europa Intex® 84 Styrene - Butadiene Copolymer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Intex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Intex® 84 Styrene - Butadiene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Intex® 084 is an aqueous anionic dispersion of a styrene-butadiene copolymer with low solid content obtained by emulsion polymerization using fatty acid soap as emulsifier. It does not contain any antioxidant.Key Features: Intex® 084 can be blended with VPL and natural latexMain Applications: Intex® 084 is mainly used for fabric impregnation and tire cord dipping.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Solids Content 41 %
41 %
Total; ISO 124
pH 11
11
ISO 976
Brookfield Viscosity 40 cP
40 cP
60 rpm; ISO 1652
Chemical Properties Metric English Comments
Styrene Content 24 %
24 %
Bound; Internal method