Polimeri Europa KOBLEND HI 41 F1 PBT+PC, Impact Grade  (discontinued **)

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa KOBLEND HI 41 F1 PBT+PC, Impact Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Symbol according to ISO 1043/1: PBT+PC-HI Similar to KOBLEND HI 41 with improved fluidity. Main application fields: bumpers Unfilled. Suitable for Injection Molding. Supplied as pellets.ISO data. Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
Melt Flow 4.3 g/10 min

@Load 2.16 kg,
Temperature 250 °C
4.3 g/10 min

@Load 4.76 lb,
Temperature 482 °F
cm³/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 47.0 MPa
6820 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal
Elongation at Yield 4.4 %
4.4 %
50 mm/min
Tensile Modulus 2.05 GPa
297 ksi
1 mm/min
Izod Impact, Unnotched NB
NB
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Izod Impact, Notched (ISO) 47.0 kJ/m²

@Temperature -30.0 °C
22.4 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
Vicat Softening Point 116 °C
241 °F
50°C/hr; 50N
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Comparative Tracking Index 400 V
400 V