Polimeri Europa KOBLEND HI 75 PBT+PC, Impact Grade  (discontinued **)

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa KOBLEND HI 75 PBT+PC, Impact Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Symbol according to ISO 1043/1: PBT+PC-HI Elastomer modified PBT+PC blend with good impact behaviour, good dimensional stability, good stiffness, resistant to solvents. Main application fields: automotive industryUnfilled. Suitable for Injection Molding. Supplied as pellets.ISO data. Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Melt Flow 2.1 g/10 min

@Load 2.16 kg,
Temperature 250 °C
2.1 g/10 min

@Load 4.76 lb,
Temperature 482 °F
cm³/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal
Elongation at Yield 5.5 %
5.5 %
50 mm/min
Tensile Modulus 2.15 GPa
312 ksi
1 mm/min
Izod Impact, Unnotched NB
NB
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Izod Impact, Notched (ISO) 44.0 kJ/m²

@Temperature -30.0 °C
20.9 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Vicat Softening Point 125 °C
257 °F
50°C/hr; 50N
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in