Polimeri Europa KOSTIL B366 Styrene Acrylonitrile

Category Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Molded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name KOSTIL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa KOSTIL B366 Styrene Acrylonitrile.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Symbol according to ISO 1043-1: SAN Grade designation according to ISO 4894-SAN 2,M,105-25 Injection moulding grade with good chemical resistance and easy flow grade Application fields: household and small appliances large appliances (internal parts) cosmetics, medical and pharmaceutical items lighting bathroom furnishing others (catering, stationery, toys, displays) Unfilled. Suitable for Injection Molding, Profile Extrusion. Supplied as pellets. Contains release agent.ISO data.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
Melt Flow 30 g/10 min

@Load 10.0 kg,
Temperature 220 °C
30 g/10 min

@Load 22.0 lb,
Temperature 428 °F
cm³/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 66.0 MPa
9570 psi
5 mm/min
Elongation at Break 2.2 %
2.2 %
5 mm/min
Tensile Modulus 3.50 GPa
508 ksi
1 mm/min
Charpy Impact Unnotched 1.60 J/cm²
7.61 ft-lb/in²
1.60 J/cm²

@Temperature -30.0 °C
7.61 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C

@Temperature 20.0 °C
38.9 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
183 °F
Vicat Softening Point 105 °C
221 °F
50°C/hr; 50N
Glass Transition Temp, Tg 103 °C
217 °F
10°C/min test
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Manufacturer specifies 'transparent' but doesn't quantify.
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm