Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Riblene® MQ 10 R Low Density Polyethylene - Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Riblene® MQ 10 R Low Density Polyethylene - Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Riblene MQ 10 R is a good fluidity low density polyethylene resin (LDPE).Parts made with Riblene MQ 10 R are characterized by a high flexibility.Main Applications: Riblene MQ 10 R is suitable for injection molding and compound applications. Riblene MQ 10 R is recommended for stoppers, closures and low thickness articles.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.918 g/cc
0.918 g/cc
ISO 1183
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 190 °C
15 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 46
46
ISO 868/A
Tensile Strength, Yield 10.0 MPa
1450 psi
ISO 527
Flexural Modulus 0.120 GPa
17.4 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 108 °C
226 °F
Internal method
Vicat Softening Point 84.0 °C

@Load 1.00 kg
183 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -40.0 °C
<= -40.0 °F
ASTM D746
Users viewing this material also viewed the following: