Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Riblene® MR 30 Low Density Polyethylene - Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Riblene MR 30 is a high fluidity low density polyethylene resin (LDPE) characterized by a high flowability and a medium rigidity.Parts made with Riblene MR 30 are characterized by good mechanical and optical properties.Main Applications: Riblene MR 30 is ideal for injection molding applications. Riblene MR 30 is recommended for houseware, high gloss toys and low thickness articles. Because of its fluidity, Riblene MR 30 is also recommended for masterbatches production.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.924 g/cc
0.924 g/cc
ISO 1183
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
ISO 868/A
Tensile Strength, Yield 12.0 MPa
1740 psi
ISO 527
Flexural Modulus 0.180 GPa
26.1 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 111 °C
232 °F
Internal method
Vicat Softening Point 92.0 °C

@Load 1.00 kg
198 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -15.0 °C
<= 5.00 °F
ASTM D746