Polimeri Europa Riblene® MT 10 Low Density Polyethylene - Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Riblene® MT 10 Low Density Polyethylene - Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Riblene MT 10 is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MT 10 are highly flexible.Main Applications: Riblene MT 10 is suitable for injection molding applications. Riblene MT 10 is recommended for low thickness articles, artificial flowers and masterbatches.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.917 g/cc
0.917 g/cc
ISO 1183
Melt Flow 40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 43
43
ISO 868/A
Tensile Strength, Yield 9.00 MPa
1310 psi
ISO 527
Flexural Modulus 0.110 GPa
16.0 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 106 °C
223 °F
Internal method
Vicat Softening Point 82.0 °C

@Load 1.00 kg
180 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -10.0 °C
<= 14.0 °F
ASTM D746