Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Cast
Manufacturer Polimersan Plastics
Trade Name POLIKES®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
POLIKES® PA6 G (CAST POLYAMIDE) is a plastic with high physical, electrical and chemical resistance. Its resistance is high especially against strokes and loads. Its temperature resistance is high, whereas corrosion coefficient is low. But, because of its water absorption property, it is not recommended at humid environments(%6-7).PROPERTIES OF POLIKES®:100°C Service TemperatureLow Corrosion CoefficientVery High Pressing ResistanceHigh HardnessHigh Resistance To StrokesResistance To HeatResistance To Chemical SubstancesLower Water Absorption compared to PA 6GENERAL USAGE AREAS OF POLIKES®:SledgesWheelsRollsGearsBearingsBobbinsHoopsCorrosion PlatesFood Industry PartsChemical Industry PartsPaper Industry PartsTextile Industry PartsPress Industry Parts Information provided by Polimersan Polimer Kimya San.Tic.Ltd.Sti.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ISO.1183 DN.53479
Water Absorption 6.0 - 7.0 %
6.0 - 7.0 %
ISO.62 DN.53495
Mechanical Properties Metric English Comments
Hardness, Rockwell M 88
88
ISO.2039-2
Hardness, Shore D 85
85
DN.53505
Ball Indentation Hardness 110 - 160 MPa
16000 - 23200 psi
ISO.2039-2
Tensile Strength at Break 88.0 - 90.0 MPa
12800 - 13100 psi
ISO.527 DN.53455
Tensile Strength, Yield 55.0 - 85.0 MPa
7980 - 12300 psi
ISO.527 DN.53455
Elongation at Break 10 - 40 %
10 - 40 %
ISO.527 DN.53455
Modulus of Elasticity 3.90 - 4.20 GPa
566 - 609 ksi
ISO.178 DN.53452
Thermal Properties Metric English Comments
CTE, linear 80.0 - 90.0 µm/m-°C

@Temperature 20.0 °C
44.4 - 50.0 µin/in-°F

@Temperature 68.0 °F
DN.53752
Melting Point 190 °C
374 °F
Maximum Service Temperature, Air 100 °C
212 °F
ISO.75 DN.53461
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
ISO.167 DN.53482
Surface Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
ISO.167 DN.53482
Dielectric Strength 80.0 - 100 kV/mm
2030 - 2540 kV/in
ISO.243 DN.53481