Material Notes:
Moplen HP425J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. MIRAEPOL T28C is a homopolymer particularly suitable for BOPP (Tender) film. Moplen HP425J resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 178.2010 for food packaging substances with adequate additives. And contains no dangerous substances according to Federal Regulations in 21 CFR 177.1520.Features: Excellent Processability and stretchability; High Transparency and Gloss; High Stiffness and Strength; Good Barrier Properties; Excellent MetallizabilityApplications: Thin gauge BOPP film; Cigarette film Information provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 98
98
ASTM D785
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.57 GPa
228 ksi
ASTM D790
Izod Impact, Notched 0.490 J/cm
0.918 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ASTM D648
Vicat Softening Point 153 °C
307 °F
ASTM D1525